Instruction Details
- Temperature:
- 400°F / 204.44°C
- Time:
- 60 seconds
- Pressure:
- Light
- Substrate:
- MPB001-PAD-A, MPB001-A (Part numbers may vary by distributor)
Heat Press Method Instructions
1. Cover the bottom table of the press with a sheet of protective paper.
2. Secure transfer to substrate using Adhesive Spray.
3. Place substrate face up, with attached transfer face down, on top of protective paper on bottom table.
4. Top with protective paper and press according to time, temperature, and pressure above.
The MPB001-A is slightly larger than the MPB001-A before imaging. The MPB001-A will shrink slightly and will fit after imaging. If product doesn't shrink to fit, flip face down and repress for an additional 30 seconds.
If the bottom pad is warped, set on flat surface until it flattens.
Stack Order for Heat Press
- HEAT PRESS PLATEN
- PROTECTIVE PAPER
- TRANSFER
- SUBSTRATE
- PROTECTIVE PAPER
- BOTTOM TABLE